Dear all,
A hydro treating reactor internals made of AUSTENITIC SS. I want to know that what is the effect of oxygen and nitrogen on AUSTENITIC SS.
The process is about removal of selfur and nitrogen from kerosene.
I ask all this because during catalyst change over , reactor internals are coated by solution of Na2CO3.
|
Austenetic Stainless Steel,metallurgy,
Started by VIrendra20911, Sep 27 2016 09:27 PM
2 replies to this topic
Share this topic:
Similar Topics
Metallurgy Of Steam Condensate SystemStarted by Guest_Vegeta_* , 09 Jan 2023 |
|
|
||
Cost Factor/index Table For Mocs Like Carbon Steel, Glass Etc.Started by Guest_daraj_* , 29 Aug 2021 |
|
|
||
Spark Potential Stainless SteelStarted by Guest_kangas_* , 03 Jun 2021 |
|
|
||
Metallurgy For Calciner Handling Chlorided Ccr CatalystStarted by Guest_abhivmairal_* , 23 Mar 2021 |
|
|
||
Temperature Profile Through Stainless.Started by Guest_LittleFish_* , 17 Nov 2020 |
|
|