Dear sirs
Could anyone sharing about experience to solve corrosion under deposition at trim cooler of overhead main fractionator?
Coolers lay out ( A to H) and opened every TA (3 years period) and found much deposit at B and G, H and thickness reduction to lower than minimum requirement
We are using corrosion inhibitor with 9 - 13 ppm from Chimec supplier